A burner liner datum setup opens two Ø8H7 holes in the base plate first, then cuts every face and hole from that one chain to 0.05 mm flatness target (0.05–0.10 mm acceptance) and ±0.05 mm hole position (ISO 2768-1). A printed liner reaches assembly because one datum chain, not the mold, carries every cut. The route removes the tooling step that casting needs and replaces the tooling reference with a datum. Two thermal cycles stand between the blank and the first cut, and the stock map accounts for both. A liner that misses that map is scrapped before the finish pass, which is why the datum is agreed before the print is released.
A printed liner wins when the wall carries windows, bosses and a datum that sheet welding cannot hold. Welding a 1.8 mm nickel wall into a liner leaves a seam at every joint, and each seam moves during the solution treatment that the assembly needs. Printing makes the same geometry in one piece, so the datum chain starts from a single blank.
The comparison is not abstract. A welded liner needs fixtures for each seam, a straightening step after welding, and a second setup after heat treatment. A printed liner needs one set of datum holes and one machining chain, which is why the route is quoted as a chain rather than as a part.
The route also sets the batch logic. Casting pays for a pattern once and then runs cheap parts; printing pays per part and skips the pattern (ASM Handbook Vol. 7). Under about 20 parts, the pattern cost dominates, and the printed route is the shorter purchase order.
Our superalloy 3D printing route covers the blank and the stress relief that follows it, so the machining step starts from a blank whose thermal history is already known. The CNC machining step then cuts every feature from one datum. Route comparisons for other liner shapes are collected on the Neway blogs page, each one quoted as a chain rather than as a part.
Three things settle before a cutter touches the blank: the datum holes, the stock map and the inspection plan. Each one has a number, and the numbers are agreed in the drawing review rather than discovered at the machine. The plan also names the inspection gate: the flatness and position readings that stop the batch if they fail, rather than readings taken for information only.
In a burner liner datum setup, the datum holes come first because every other feature is measured from them. Two Ø8H7 holes in the base plate, 0.02 mm true position, give the fixture a repeatable location without touching the printed skin. The base plate flatness has to reach 0.03 mm before those holes are opened, or the datum itself is cut from a warped face.
Feature | Allowance or callout | Check before release |
|---|---|---|
Base plate flatness | 0.03 mm | Surface plate, dial indicator |
Datum holes (2 × Ø8H7) | 0.02 mm true position | CMM |
Assembly faces | 2.0 mm stock | Post-HIP scan |
Holes | 1.0 mm stock | Pre-machining scan |
Final flatness | 0.05 mm target, 0.05–0.10 mm acceptance | Surface plate after unclamping |
The stock map and the inspection plan follow the datum. The stock map is read from the post-HIP scan, not from CAD, because the two thermal cycles move the blank by up to 0.5 mm. The inspection plan names the instrument for each row of the table above, and the plan is signed before the first cut so the operator is not inventing acceptance limits at the machine.
The burner liner datum setup is built in two operations: open the datum and cut the plate in operation one, then cut every remaining face and hole from that datum in operation two. The printed skin never becomes a datum, because it is the surface that moves.
Operation one faces the base plate to 0.03 mm, drills and reams the two Ø8H7 holes, and marks the reference edge. The plate is clamped on a soft jaw at no more than 0.5 MPa, because the 1.8 mm wall behind it stores clamp load that releases as a bow after unclamping.
Operation two bolts the part on the two holes and cuts the assembly faces, the window frames, the Ø12 holes and the M4 threads. Every position in this operation is a distance from the datum holes, so a 0.05 mm move at the datum becomes a 0.05 mm move at the bolt circle. The fixture is the same fixture for all three trial parts, which is what makes the third-part comparison meaningful. The reference edge is marked so the second operation loads the same way on every part.
The chain is checked upward at the end. Flatness is read on a plate after unclamping, position is read on a CMM, and the two readings are compared with the scan that went in. If the flatness drifted but the position held, the wall released; if both drifted, the datum moved. The same fixture cuts the three trial parts, because a fixture that changes between parts cannot separate fixture error from process error.
Faces carry 2.0 mm and holes carry 1.0 mm, measured from the post-HIP scan. The face allowance covers the datum cut, 0.05 mm of flatness and the local warp; the hole allowance covers position, which moves with the thermal cycles and with the stress released by the face cut.
The allowance is not uniform. Window frames and ribs move less than the long open wall, so 2.0 mm is a minimum over the part, not a target. A region that prints 1.6 mm out of nominal is already at the edge, and the answer is a second look at orientation, not more stock.
More stock stops helping at about 3.0 mm on the faces. Beyond that, the extra metal has to be removed in a second roughing setup, the part is handled twice, and the thicker pad cools more slowly than the 1.8 mm wall, which makes the heat treatment gradient a distortion source of its own.
The heat treatment and the hot isostatic pressing step are measured against the same stock map. Solution treatment at 1,180 °C for 1 h releases printing stress, and HIP at 1,180 °C and 100 MPa for 3 h closes porosity and creeps the wall; together they can move the blank by 0.5 mm, which is why the allowance is read from the scan after both and never from CAD. The scan is taken with the datum holes already in place, so the allowance is measured from the surface the cutter will actually use.
The wall is held by spreading the clamp load over a soft jaw and filling the cavity with plaster, not by adding pressure. A three-jaw chuck on a 1.8 mm wall punches a local dent that turns into a flatness error after unclamping.
Soft jaws are milled to the part contour, so the load lands on an area rather than a point, and the pressure stays at or below 0.5 MPa. The plaster core supports the inside of the shell, damps vibration and carries part of the clamp load, and it is broken out and washed after machining.
Cutting parameters follow the material. A 0.1 mm radial depth in the finishing pass keeps the tool engaged without pulling the wall, and a sharp edge with a positive rake stays in the cut instead of rubbing. The powder bed fusion blank that arrives at this step already has its stress relief behind it, so the cut is not opening a locked-in stress field in the same way a welded wall would.
Where the wall cannot be supported, the process changes rather than the force. Two setups with a release and a check in between, extra stock for a light final pass, or a datum on a thicker feature are the three options, and each one is named in the quote so the choice is visible. Where a slot is too deep for a cutter, EDM removes it after the datum cuts, and surface treatment is chosen only after the finish pass.
The printed blank stops being worth machining below a 0.6 mm wall, above about 200 parts, or when the geometry needs a certification route that the print cannot carry. Below 0.6 mm the clamp and the cut both dominate the tolerance, and the wall moves more than the stock can cover.
Above 200 parts the pattern cost of casting is absorbed, and a casting with a machining allowance becomes the cheaper route per part. The printed route still wins when the casting lead time blocks an assembly date, but that is a schedule argument, not a cost argument, and it should be stated as one. The stock map stays valid for the batch it was measured on, not for the next blank from a new build.
Inside the printable range, the chain is what holds the result. Outside it, the honest answer is a different route: a casting with a machining allowance, a welded assembly with a straightening step, or a machined solid when the batch is small enough to justify it.
Two Ø8H7 holes at 0.02 mm true position, 2.0 mm face stock, 0.5 MPa clamp load and 0.05 mm flatness after unclamping are the numbers this route repeats on a 1.8 mm GH3536 wall.
Send the drawing with the datum callout, the wall thickness and the batch size. Neway reviews the datum chain against your assembly, returns the stock map and quotes the superalloy 3D printing and CNC machining steps together, with the inspection gate named. A titanium or stainless route is quoted only where the duty calls for it.