First-Article Trial Cut: How Do You Prove Stability?

Table of Contents
What does the first-article trial cut prove?
Which dimensions go on the record?
When is the process stable enough to release?

A first-article trial cut proves a printed liner by running three parts through the same setup, not one. The same 12 dimensions are measured on each part, the spread is compared with the 0.05 mm flatness callout, and the process is released only when the third part adds no new failure. One part shows what the machine can do; three show what it repeats.

What does the first-article trial cut prove?

One part proves the program, not the process. It shows that the tool reaches the surfaces, that the fixture holds the part, and that the probe agrees with the drawing. It does not show whether the next part holds the same tolerance, or whether the fixture repeats after a part change. The first-article trial cut is judged on three parts, and the record names all three.

Three parts are the practical minimum because the two thermal cycles move each blank differently. The first part carries the most stock, up to 2.0 mm on the faces, and the most heat; the second and third see the setup after the fixture has settled. A process that only holds on part one will fail in the batch. Each part keeps its own scan and its own record, and the three records are compared side by side rather than averaged.

The trial is run to production parameters, not to a safe set. Spindle speed, feed and depth of cut are the values the batch will use, and the fixture is the fixture that will be used. A trial on a light pass proves nothing about the finish cut.

Which dimensions go on the record?

The record carries 12 dimensions: flange face flatness, two datums, four hole positions, three wall thicknesses and the bore diameter. Each is measured on all three parts, at the same points, after the same thermal history. The record names the instrument, the operator and the room temperature.

Flatness is measured on a surface plate with a dial indicator, and the reading is the maximum minus the minimum over the face, not a single point. Position is checked with a CMM or a fixture gauge, and the value is the true position, not the distance from an edge. The indicator is zeroed on the plate, not on the part, and each face is read in at least five positions.

The record also carries the blank scan and the post-HIP scan, so movement from heat is separated from movement from the cutter. Without that pair, a drift in flatness can be blamed on the machine when it came from the furnace.

When is the process stable enough to release?

The process is stable enough to release when the third part adds no new failure and the spread of the 12 dimensions is inside 60 percent of the tolerance. For 0.05 mm flatness that means a spread of 0.03 mm across three parts, not one part under 0.05 mm. A trend across the three parts is a fail even when every value is inside tolerance, because the fourth part will follow the trend.

A capability number supports the release. With three parts, Cp is only indicative, so it is reported as a range and read with the spread. A Cp above 1.33 on the recorded dimensions, with no trend across the three parts, is the usual gate.

The release also names what is not proven. A three-part run does not prove tool life, and it does not prove the process at the end of a 20-part batch. The record states the batch size the release covers and the interval for the next check. A tight spread allows a longer interval; a wide one requires a check every five parts.

Send the drawing, the tolerance callout and the batch size. We will run the first-article trial cut, record the 12 dimensions against the scan, and quote the CNC machining and superalloy printing steps with the stability record. One review covers the fixture, the heat treatment and the HIP sequence. Include the inspection report format your quality team uses.