English

What G1/8 Thread Depth Fits a Transition Duct Boss?

Table of Contents
Why tap G1/8 instead of printing the thread?
What pilot hole sets G1/8 thread depth?
When does a shallow thread fail the gauge?

G1/8 thread depth on a printed transition duct boss is 21.12 mm into a ⌀8.8 mm pilot hole, tapped at 300 r/min. The pilot runs 26.4 mm through the 6 mm boss and the 2.5 mm wall, so the tap has a clear exit and full engagement at the port face. Depth is set from the boss face rather than from the far side of the wall, and the gauge is read against ISO 228-1.

Why tap G1/8 instead of printing the thread?

A printed G1/8 thread does not hold its pitch or its flank angle on a 2.5 mm wall. Laser powder bed fusion leaves a stair-step surface on a 55° flank, and the pitch over 21.12 mm drifts enough that a fitting binds part way in. Tapping after the boss face is cut puts the thread on a machined axis instead of on a printed skin.

Tapping also keeps the thread tied to the machined datum. The tap follows the pilot bore that was cut from the spigot datum, so the thread axis and the boss axis stay inside ⌀0.20 mm. A printed thread would carry the 0.5 mm of ovality that solution treatment leaves in the shell, and the fitting would sit off-centre on the port face.

The limit is engagement length, not thread size. When a boss cannot give 21.12 mm of usable depth, the design needs a taller boss or an insert, and no tapping plan fixes a short boss. The CNC post-machining plan therefore starts from the boss height, not from the thread callout.

What pilot hole sets G1/8 thread depth?

The pilot finishes at ⌀8.8 × 26.4 mm through, which sets the G1/8 thread depth at 21.12 mm below the boss face. The blank arrives at ⌀8.4 mm, so 0.2 mm of radial stock goes to the boring bar before the tap enters. Boring the pilot is part of the same powder bed fusion route that produced the blank.

Boring and tapping share one setup with the boss faces. Opening the fixture between bore and tap adds close to 0.2 mm of spread on a 2.5 mm wall, which is twice the coaxiality the thread is allowed. The fixture holds 0.4 MPa on the spigot land rather than on the shell, so the wall does not spring between the two operations.

Speed is fixed rather than chosen by the operator. The tap runs at 300 r/min in a rigid holder, and the hole is cleared of chips before the tap starts. A chip packed inside a 26.4 mm through hole lifts the gauge reading and looks like a shallow thread.

When does a shallow thread fail the gauge?

G1/8 thread depth is accepted only when the go plug passes and the no-go stops at 21.12 mm. A plug that bottoms out early means the thread is shallow, and the boss goes back to the tap rather than to the CMM. The check runs on every part, not on a sample of the batch.

The gauge reads depth and form together. A thread cut with a worn tap can pass depth and still fail the no-go at the flank, so both ends of the gauge are read before a boss is released. Thread depth alone does not release a port.

Two other numbers come off the same setup. The thread axis has to stay within ⌀0.20 mm of its boss, and the port face has to sit at 6.0 mm above the duct axis. Both are read from the datum chain that runs from the two spigots to the eight boss faces.

Two cases sit outside this answer. A boss already welded to close a cleaning hole cannot be re-tapped to depth, because the weld changes the flank support under the thread. A port that carries a customer thread class is judged against that drawing, not against this article.

A shallow thread is re-tapped once. A second re-tap on the same boss removes flank material, and the no-go starts to pass, so a boss that fails twice goes to review rather than back to the tap. The gauge proves the thread form and nothing else: it does not prove that a fitting will hold pressure, because sealing depends on the port face and on the fitting, and this part carries no pressure test.

Send the boss pattern, the port callout and the thread class to Neway, and we will set the pilot diameter, the depth from the boss face and the gauge plan for each of the eight ports. The same review covers the CNC machining step that bores and taps the ports and prices the superalloy 3D printing blank behind it.