English

Boss Stock Allowance on a Transition Duct Print?

Table of Contents
How much stock does a 6 mm boss need?
Why does boss stock allowance differ by face?
When is more stock the wrong answer?

Boss stock allowance on a printed transition duct is 1.0 mm on the boss faces and 0.4 mm in the pilot holes. The 2.5 mm wall moves in the furnace, so stock has to cover that movement rather than only the tool marks the printer leaves. Faces and holes carry different numbers because one is a flat face and the other is a bore with a thread behind it.

How much stock does a 6 mm boss need?

A boss 6 mm tall takes 1.0 mm on its face. The face is the thread seat and the port datum, so it is cut flat and clean in one operation after the furnace run. A thinner allowance leaves no material when the wall bows by 0.5 mm and the face has to come back to 6.0 mm above the axis.

Holes carry 0.4 mm on diameter rather than on radius. A ⌀8.8 mm pilot arrives at ⌀8.4 mm, and the boring bar removes 0.2 mm per side. That is enough for one pass to clean the printed stair-step and still leave the thread with 21.12 mm of usable depth behind the face.

Both numbers of the boss stock allowance come off the same CNC machining setup. Cutting the faces first and the holes second in one clamp keeps the port and the thread seat on one datum, and it is the reason the two allowances are specified together rather than face by face.

Why does boss stock allowance differ by face?

Faces and bores fail for different reasons. A face loses its allowance to a bow across the part, while a bore loses its allowance to a shift along the wall. A single number for both would either over-machine the face or leave the bore too tight to clean.

The furnace sets the size of the bow. Solution treatment at 1180 °C with 2 bar argon cooling leaves up to 0.5 mm of ovality in the 2.5 mm shell, and the boss feet move with it. When the face is cut from the spigot datum, that movement appears as stock, and 1.0 mm absorbs it without cutting into the boss root.

The bore reacts to a different error. Printing leaves the pilot about 0.15 mm off its nominal position, so the machine has to re-cut the position as well as the surface. Boring from the datum takes that shift out in one pass, and the datum chain is what makes the second pass unnecessary.

When is more stock the wrong answer?

More stock stops helping when the extra material changes how the part cools. A 2.0 mm face allowance on a 6 mm boss turns the boss into a thick section that cools at a different rate from the 2.5 mm wall, and the cast of the boss foot becomes the error instead of the cure. The stock has to stay small enough that the boss and the wall still cool as one shell.

Boss stock allowance also has a cost. Every extra millimetre is cut at a layered step of 0.3 mm with the fixture holding 0.4 MPa on the spigot, so a thicker allowance adds passes without adding accuracy. The allowance is sized to the movement, not to the operator's comfort.

Two limits sit outside this answer. A duct with a wall below 1.0 mm cannot carry 1.0 mm of face stock, because the boss root would be thinner than the stock after the cut. A part that has to be machined in two clamps cannot hold the same allowance, and the second clamp usually needs 0.2 mm more to absorb the re-datum.

A third case is a part that needs no stock at all: a boss that is machined from solid stock does not carry printed stock, and the allowance rule then belongs to the supplier of the bar, not to the print. Mixing the two routes on one duct is what produces the argument about allowances in the first place.

Send the boss layout, the furnace cycle and the datum plan to Neway, and we will confirm the allowance on each face and each bore before the first cut. The same review covers the superalloy 3D printing blank and the CNC post-machining that follows it.